Brand Name : Torich

Model Number : A358/A358M

Certification : TS16949 , BV , ABS , CCS , DNV

Place of Origin : China

MOQ : 5MT

Price : negotiable

Payment Terms : L/C, T/T

Supply Ability : 7000MT/Month

Delivery Time : 30~35days

Packaging Details : In bundles or in wooden box

Product Name : Stainless Steel Tube

Application : For High-Temperature Service

Grade : 201 , 304/304L , 310S , 316/316L , 317/317L

Production : Welded

Contact Now

A358/A358M Austenitic Chromium-Nickel Alloy Stainless Steel Pipe for High Temperature

ASTM A358/A358M

Electric-Fusion-Welded Austenitic Chromium-Nickel
Stainless Steel Pipe for High-Temperature Service

Grade:

316L, 317, 317L, 321, 321H, 348

S32050, N08800.

Welding:

The joints are full penetration bouble-welded or single-welded

Heat treatment:

All pipes are with heat treatment condition.

Please specify your heat treatment requirement in the enquiry.

Permissible Variations—The dimensions at any point in a length of pipe shall not exceed the following:

Outside Diameter—Based on circumferential measurement, 60.5 % of the specified outside diameter.

Out-of-Roundness—Difference between major and minor outside diameters, 1 %.

Alignment—Using a 10-ft [3-m] straightedge placed so that both ends are in contact with the pipe, 1⁄8 in. [3 mm] deviation from contact with the pipe.

Thickness—The minimum wall thickness at any point in the pipe shall not be more than 0.01 in. [0.3 mm] under the nominal thickness.

Table 1 Annealing Requirements

Grade or UNS DesignationA

Heat Treating

TemperatureB

Cooing/Testing

Requirements

All grades not individually listed below:

304H,309S,309Cb,310S,310Cb,321H,347H,S22100, S28300

1900 °F [1040 °C]

C

1900 °F [1040 °C]

D

N08020

1800-1850 °F [980-1010 °C]

D

N08367

2025 °F [1110 °C]

D

N08810

2050 °F [1120 °C]

D

N08904

2000 °F [1095 °C]

D

N08926

2010 °F [1100 °C]

D

S30600

2100 °F [1150 °C]

D

S30815

1920 °F [1050 °C]

D

S31254

2100 °F [1150 °C]

D

S31266

2100 °F [1150 °C]

D

S31727

1975–2175 °F [1080 to 1180 °C]

D

S32050

2100 °F [1150 °C]

D

S32053

1975–2175 °F [1080 to 1180 °C]

D

S32654

2100 °F [1150 °C]

D

S34565

2050 °F [1120 °C]

D

A New designation established in accordance with Practice E527 and SAE J1086.

B Minimum, unless otherwise stated.

C Quenched in water or rapidly cooled by other means, at a rate sufficient to prevent reprecipitation of carbides, as demonstrable by the capability of passing Practices

A262, Practice E. The manufacturer is not required to run the test unless it is specified on the purchase order (see Supplementary Requirement S7). Note that Practices

A262 requires the test to be performed on sensitized specimens in the low-carbon and stabilized types and on specimens representative of the as-shipped condition for

other types. In the case of low-carbon types containing 3 % or more molybdenum, the applicability of the sensitizing treatment prior to testing shall be a matter for

negotiation between the seller and the purchaser.

D Quenched in water or rapidly cooled by other means.

Inspection and Quality Control:

In house control, also accept Customer Inspection at site or Third Party Inspection

High Temperature Chromium Nickel Alloy Tube A358 / A358M Welded Stainless Steel Pipe High Temperature Chromium Nickel Alloy Tube A358 / A358M Welded Stainless Steel Pipe

Referenced Documents:

ASTM Standards:

ASTM A240/A240M Specification for Chromium and Chromium Nickel Stainless Steel Plate, Sheet, and Stip for Pressure Vessel and for General Application

ASTM A262 Practices for Detecting Susceptibility to Intergranular Attack in Austenitic Stainless Steels

ASTM A480/ A480M Specification for General Requirements for Flat-Rolled Stainless and Heat-Resisting Steel Plate, Sheet, and Strip

ASTM A941 Terminology Rlating to Steel, Stainless Steel, Related Alloys and Ferroalloys

ASTM A999/A999M Specification for General Requirements for Alloy and Stainless Steel Pipe

E527 Practice for Numbering Metals and Alloys (UNS)


Product Tags:

nickel alloy pipe

      

heat exchanger tubes

      
Wholesale High Temperature Chromium Nickel Alloy Tube A358 / A358M Welded Stainless Steel Pipe from china suppliers

High Temperature Chromium Nickel Alloy Tube A358 / A358M Welded Stainless Steel Pipe Images

Inquiry Cart 0
Send your message to this supplier
 
*From:
*To: TORICH INTERNATIONAL LIMITED
*Subject:
*Message:
Characters Remaining: (0/3000)
 
Inquiry Cart 0